Low temperature spark plasma sintering of YIG powders

AuthorsFernández-García, Lucía ; Suárez, Marta ; Menéndez, José Luis
KeywordsCeramic
Magnetically ordered materials
Sintering
Magnetization
Optical spectroscopy
Magnetic measurements
Issue DateJul-2010
PublisherElsevier
CitationJournal of the European Ceramic Society 502(1): 132-135 (2010)
AbstractA transition from a low to a high spin state in the magnetization saturation between 1000 and 1100 °C calcination temperature is observed in YIGpowders prepared by oxides mixture. Sparkplasmasintering of these powders between 900 and 950 °C leads to dense samples with minimal formation of YFeO3, opening the way to co-sintering of YIG with metals or metallic alloys. The optical properties depend on the sintering stage: low (high) density samples show poor (bulk) optical absorption.
Description4 páginas, 4 figuras, 2 tablas.
Publisher version (URL)http://dx.doi.org/10.1016/j.jallcom.2010.04.117
URIhttp://hdl.handle.net/10261/48233
DOI10.1016/j.jallcom.2010.04.117
ISSN0955-2219
Appears in Collections:(CINN) Artículos
Files in This Item:
File Description SizeFormat 
Low temperature spark.pdf433,47 kBAdobe PDFThumbnail
View/Open
Show full item record
Review this work
 

Related articles:


WARNING: Items in Digital.CSIC are protected by copyright, with all rights reserved, unless otherwise indicated.