Formation of nitrile species on Ag nanostructures supported on a-Al2O3: a new corrosion route for silver exposed to the atmosphere

AutorPeláez, Ramón J. CSIC ORCID; Espinós, J.P. CSIC ORCID; Afonso, Carmen N. CSIC
Palabras claveSilver
Metal nanoparticles
Oxidation
Corrosion
Pulsed laser deposition
Fecha de publicación2017
EditorInstitute of Physics Publishing
CitaciónNanotechnology, 28: 175709-175723 (2017)
ResumenThe aging of supported Ag nanostructures upon storage in ambient conditions (air and room temperature) for 20 months has been studied. The samples are produced on glass substrates by pulsed laser deposition (PLD); first a 15 nm thick buffer layer of amorphous aluminum oxide (a-Al2O3) is deposited, followed by PLD of Ag. The amount of deposited Ag ranges from that leading to a discontinuous layer up to an almost-percolated layer with a thickness of <6 nm. Some regions of the as-grown silver layers are converted, by laser induced dewetting, into round isolated nanoparticles (NPs) with diameters of up to ∼25 nm. The plasmonic, structural and chemical properties of both as-grown and laser exposed regions upon aging have been followed using extinction spectroscopy, scanning electron microscopy and x-ray photoelectron spectroscopy, respectively. The results show that the discontinuous as-grown regions are optically and chemically unstable and that the metal becomes oxidized faster, the smaller the amount of Ag. The corrosion leads to the formation of nitrile species due to the reaction between NOx species from the atmosphere adsorbed at the surface of Ag, and hydrocarbons adsorbed in defects at the surface of the a-Al2O3 layer during the deposition of the Ag nanostructures by PLD that migrate to the surface of the metal with time. The nitrile formation thus results in the main oxidation mechanism and inhibits almost completely the formation of sulphate/sulphide. Finally, the optical changes upon aging offer an easy-to-use tool for following the aging process. They are dominated by an enhanced absorption in the UV side of the spectrum and a blue-shift of the surface plasmon resonance that are, respectively, related to the formation of a dielectric overlayer on the Ag nanostructure and changes in the dimensions/features of the nanostructures, both due to the oxidation process
Versión del editorhttps://doi.org/10.1088/1361-6528/aa65c0
URIhttp://hdl.handle.net/10261/148916
DOI10.1088/1361-6528/aa65c0
Aparece en las colecciones: (ICMS) Artículos
(CFMAC-IO) Artículos




Ficheros en este ítem:
Fichero Descripción Tamaño Formato
Formation_of_nitrile_Pelaez17.pdf1,47 MBAdobe PDFVista previa
Visualizar/Abrir
Mostrar el registro completo

CORE Recommender

SCOPUSTM   
Citations

1
checked on 11-abr-2024

WEB OF SCIENCETM
Citations

3
checked on 22-feb-2024

Page view(s)

280
checked on 18-abr-2024

Download(s)

40
checked on 18-abr-2024

Google ScholarTM

Check

Altmetric

Altmetric


NOTA: Los ítems de Digital.CSIC están protegidos por copyright, con todos los derechos reservados, a menos que se indique lo contrario.